In this study, the graphite/epoxy prepregs were surface-treated using oxygen plasma, and optimal treatment time was determined measuring the contact angle on the prepreg surface. Interlaminar fracture behavior of surface-treated graphite/epoxy composites was compared with that of regular (untreated) graphite/epoxy composites. The results showed that the contact angle was a minimum when treated for 30 minutes. The interlaminar fracture toughness of surface-treated specimen was improved about 15% compared with that of regular specimen.